Liquid-Phase Atomic Layer Deposition on Dispersed Materials

© 2019 LPDC
Our paper on liquid-phase atomic layer deposition was published in Advanced Materials! Liquid‐phase atomic layer deposition is performed on high‐surface‐area dispersed nanomaterials at room temperature and pressure. This new method requires typical laboratory equipment, uses no excess precursors or purging steps, and allows for easy monitoring of the reaction by quantifying ligand release.